Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations MintJulep on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Australia to close 8 GW of coal power by 2030 2

Status
Not open for further replies.
Well, that was encouraging :)

The problem with sloppy work is that the supply FAR EXCEEDS the demand
 
FYI... funny stuff... I'd not heard of it before...

Clipboard01_vftx1u.jpg


Rather than think climate change and the corona virus as science, think of it as the wrath of God. Feel any better?

-Dik
 
dik, is there any battery chemistry that isn't toxic?
NiCd, Pb-H2SO4, Li; I can't think of any offhand that I would want to dance with.

= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, consulting work welcomed
 
Well some are worse than others, but you're right, I can't think of one that isn't very bad.

In the combustion context, vanadium pentoxide is able to flux metal surfaces at temperatures as low as the 1150°F range, so attack can be rapid and catastrophic, even for high alloy materials.

"Everyone is entitled to their own opinions, but they are not entitled to their own facts."
 
Why bother with chemical batteries when you've got the totally feasible and definitely efficient Energy Vault to utilize?

- Andrew
 
Don't think anyone has mentioned the elephant in the room - coal exports to Russia's only friend.

"Everyone is entitled to their own opinions, but they are not entitled to their own facts."
 
Status
Not open for further replies.

Part and Inventory Search

Sponsor

Back
Top