I've got a specification that requires a solution anneal (1900F) with soak time of 2 hours per inch of thickness. We are typically dealing with 1/2" to 1" plate. That amount of time seems a bit excessive to me and now I know why we have a fair amount of oxidation/scale when we get these parts back. For comparison, ASME UHA-44 (Sec 8, Div 1) provides soak times on solution annealing after strain hardening with a soak time of 20 min/inch or 10 min, whichever is greater.
So, what duration are you guys typically specifying for a full solution anneal of austenitic stainless?