ryu.changmyong
Mechanical
Hi, Concerned person
Recently, I surprised when I heard of happening welding crack in area of stainless steel
since about 3 years of S.Steel welding in small size of 2-1/2"
When I review technical specification in feed water line where pressure is less than 50 psi.
it allowed to install pipe spool with
non-wleding method (compressing mechine) less than 2-1/2" size in order to avoid
any possible wleding crack.
so nowdays all most pipe welding below 2-1/2" pipe size is to do non-welding method.
So, I wonder that which method is more better between welding and pressing in a low pressure pipe line.
Kind regards,
ChangMyong