I want to atomize C90700 bronze bars (89%CU 11%Sn) to a relatively large particle size so that I can use it as an alloying addition for iron. I will need approximately 2000 lbs a day to treat about 500 tons of iron a day. For this to be financially feasible it would have to cost less than $2/lb.