ASTM vs ISO Material for Pipeline

Status
Not open for further replies.

nickypaliwal

Materials
Joined
Aug 28, 2014
Messages
199
Location
OM
Can we use ISO 15590-2/3 flanges and fittings inplace of F694 forgings and viceversa?

ISO looks more stringent compared to ASTM for pipeline forgings and fittings. Does it mean that most of the clients follow only ISO 15590 ?

Regards,
Nikhil
 
Yes, ISO 15590 is more stringent than its ASTM counterparts because: a) it was co-drafted by a group of oil company engineers, principally from Europe, along with US manufacturers; b) it has been subjected to a worldwide review and comment process, and not simply a US based committee process.

ASTM A694 is a fairly rudimentary specification, and if consideration would be given to an off-the-shelf alternative to ISO 15590, then it would be ASME B16.49 for induction bends, ASTM A707/MSS SP-44 for flanges, and ASTM A860/MSS SP-75 for fittings.

Steve Jones
Corrosion Management Consultant


All answers are personal opinions only and are in no way connected with any employer.
 