Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations JAE on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

ASTM to DIN equivalents 1

Status
Not open for further replies.

nlj

Materials
Joined
Sep 13, 2007
Messages
46
Location
US
Is there a place to look up DIN equivalents for ASTM steel standards? I'm looking for equivalents for ASTM A656, Grade 80 and ASTM A572, Grade 50.

Thanks!
 
nlj,

The best way to do this is to use a professionally developed reference, such as Stahlschlüssel, ASM's Worldwide Guide to Equivalent Irons and Steels, or ASTM's Handbook of Comparative World Steel Standards: Second Edition. Some suppliers of steel products have partial information on their websites, but they are not necessarily up-to-date or broad in their coverage. Here are some links that you can use to obtain these references:




Grade S550MC (1.0986) according to DIN EN 10149-2 is equivalent to ASTM A 656 Grade 80. This standard covers all flat products, not just plate, so there are some thickness restrictions on the high strength grades in the plate range (16 mm max). DIN EN 10025-4 also covers structural plates in HSLA grades, but the highest strength available is S460ML (1.8838) which is roughly equivalent to ASTM Grade 70. Producers such as voestalpine Grobblech produce higher strength plate using their tradename alform® (alform 550 M would be Grade 80). Grade S355GP according to DIN EN 10248-1 is equivalent to ASTM A 572 Grade 50 for structural shapes, piling, etc. Use the following links for more information:




 