ASTM A-540 requires the mechanical tests to be conducted in accordance with the Methods and Definitions in A-370. Para 11.2 of A-370 allows the use of proportional small sized specimens as shown in the noted figure.
When A-540 production pieces are too small to yield a standard sized specimen, are the proportional small sized specimens prohibited in A-540 or A-370?
 
Replies continue below

Recommended for you

No.
But I get very angry when a lab uses a sub-sized sample and does not state it on the report.

= = = = = = = = = = = = = = = = = = = =
Plymouth Tube
 
I agree with Ed. On both counts.
 
There is a similar thread over in ASME Code Issues.
When you send a test piece out are you requiring a full size specimen?
 