Dear all,

Could you give me advice: where we can order glass cradle for specimen support according ASTM G48?

Thank you in advance
 
Buy glass rod and a torch and learn to make your own.
If you do much testing you will need them, and you will break them.

= = = = = = = = = = = = = = = = = = = =