I would like to be able to do ASTM G-36 (Test for evaluating SCC resistance of metals in boiling MgCl2 solution) test in-house. The test setup talks about a modified Allihn condenser along with a trap. Does anyone know where I can find these products? I am able to find the usual designs, but the modified designs as per the standard have been a problem.

Thanks
 
There used to be multiple sources selling these. Keep looking.

I believe that one modification is cutting the tail off of the condenser?
Do it yourself, glasswork isn't that hard.
I last made some of these 30 years ago so my memory is a little fuzzy on the details.

= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, Plymouth Tube
 