I need to perform hardness check on some item using a portable Hardness tester.
The test shall be in accordance to an International Standard, ASTM would be the best option.
I found two possible methods:
- impedance
- resistivity
Hardenss measure by ultrasonic contact impedance method is standardized by ASTM A1038.
Hardness measure by resistivity is standardized by DIN 50157, but is didn't find ASTM Standard/Code for it.
Does anyone know if there is an ASTM Standard for hardness measures by resistivity method?
Thank you, kind regards.
Attilio Brambilla
Material Engineer
I need to perform hardness check on some item using a portable Hardness tester.
The test shall be in accordance to an International Standard, ASTM would be the best option.
I found two possible methods:
- impedance
- resistivity
Hardenss measure by ultrasonic contact impedance method is standardized by ASTM A1038.
Hardness measure by resistivity is standardized by DIN 50157, but is didn't find ASTM Standard/Code for it.
Does anyone know if there is an ASTM Standard for hardness measures by resistivity method?
Thank you, kind regards.
Attilio Brambilla
Material Engineer