btrueblood
Mechanical
- May 26, 2004
- 10,018
Ok, it may have been done to death, but I had not heard of the ASTM F1941 and its cohort spec. F1940 before. A quick search failed to deliver a succinct answer.
If zinc plating is applied per F1941, can an ASTM A574 alloy socket head cap screw be reasonably said to be free of hydrogen embrittlement?
Or are does the standard warning (don't zinc plate on steel with tensile strength > 150 ksi) still apply?
My fallback is to specify a good zinc-rich primer paint or similar anti-corrosion coating on standard black oxide finished fasteners.
If zinc plating is applied per F1941, can an ASTM A574 alloy socket head cap screw be reasonably said to be free of hydrogen embrittlement?
Or are does the standard warning (don't zinc plate on steel with tensile strength > 150 ksi) still apply?
My fallback is to specify a good zinc-rich primer paint or similar anti-corrosion coating on standard black oxide finished fasteners.