Can some body give the salient features of the above standard (Such as Test Duration).
 
This specification identifies hardness testing and tension testing for fasteners. The hardness testing is either Brinell, Rockwell, or Vickers, and can range from approximately 30 s to 5 min. Tension testing can range from approximately 5 min to 30 min.

Regards,

Cory