ASTM F 606 What is the Test Duration

Status
Not open for further replies.

bmoorthy

Mechanical
May 29, 2003
457
Can some body give the salient features of the above standard (Such as Test Duration).
 
Replies continue below

Recommended for you

This specification identifies hardness testing and tension testing for fasteners. The hardness testing is either Brinell, Rockwell, or Vickers, and can range from approximately 30 s to 5 min. Tension testing can range from approximately 5 min to 30 min.

Regards,

Cory