hello everyone
i need to evaluate J-integral(Jc) for polymer specimen, so which convinient ASTM code i should use.
My best regards
 
Replies continue below

Recommended for you

Is not ASTM E1820 for metallic materials? I thing ASTM D 5045 or D5528 or D6671 or D7905 may be the correct standard.
 