Jan 2, 2017 #1 zerrouki Mechanical Joined Oct 8, 2015 Messages 7 Location DZ hello everyone i need to evaluate J-integral(Jc) for polymer specimen, so which convinient ASTM code i should use. My best regards
hello everyone i need to evaluate J-integral(Jc) for polymer specimen, so which convinient ASTM code i should use. My best regards
Jan 7, 2017 #2 TVP Materials Joined Apr 12, 2002 Messages 4,592 Location US ASTM E1820 Upvote 0 Downvote
Jan 17, 2017 1 #3 Cleandive Mechanical Joined Aug 3, 2014 Messages 12 Location CA Is not ASTM E1820 for metallic materials? I thing ASTM D 5045 or D5528 or D6671 or D7905 may be the correct standard. Upvote 0 Downvote