Dear All,
Please help to find the solution that we required ASTM B705 Class 1 UNS08825 (thickness 9.53 & 6.5 mm)EFW pipes for our project. As per B705 Pipe shall be made from flat-rolled alloy by an automatic
welding process with no addition of filler metal.
But, as an alternative pipe manufacturer proposing ASTM B705 Class 1 EFW pipes with addition of filler metal.
Since its deviation from the material standard, Client asking us to provide the technical justification to accept the proposal.
Please clarify, any international standards support this case
Please help to find the solution that we required ASTM B705 Class 1 UNS08825 (thickness 9.53 & 6.5 mm)EFW pipes for our project. As per B705 Pipe shall be made from flat-rolled alloy by an automatic
welding process with no addition of filler metal.
But, as an alternative pipe manufacturer proposing ASTM B705 Class 1 EFW pipes with addition of filler metal.
Since its deviation from the material standard, Client asking us to provide the technical justification to accept the proposal.
Please clarify, any international standards support this case