Hello,
I need your help for the following :
According to ASTM B444 (inconel 625 pipe and tube), the wall thickness tolerance is +/- 10% for an outside diameter tube of 0.62 in. (15.8 8mm)
But if the minimum wall is fixed to 0.05 inch (1.25 mm), what is the tolerance on the wall thickness?
Is-it -0% +10% or -0% +20%?
Thanks in advance for your help.
Nicholas.