Jul 16, 2007 #1 mikycampo Mechanical Joined Jan 3, 2007 Messages 17 Location IT dear all, i cannot find mechanical properties of ASTM A694-f60 steel i need: allowable stress (20°C) yield strength (20°C) ultimate tensile strength (20°C) young modulus thanks michele
dear all, i cannot find mechanical properties of ASTM A694-f60 steel i need: allowable stress (20°C) yield strength (20°C) ultimate tensile strength (20°C) young modulus thanks michele
Jul 16, 2007 #2 NozzleTwister Mechanical Joined Mar 3, 2003 Messages 368 Location US Per ASTM A 694/A 694M - 03 for F60... Yeild Strength (0.2% offset): 60 ksi (415 MPa) Tensil Strength: 75 ksi (515 MPa) Refer to your Design Code for allowable stresses and values for young's modulus. NozzleTwister Houston, Texas Upvote 0 Downvote
Per ASTM A 694/A 694M - 03 for F60... Yeild Strength (0.2% offset): 60 ksi (415 MPa) Tensil Strength: 75 ksi (515 MPa) Refer to your Design Code for allowable stresses and values for young's modulus. NozzleTwister Houston, Texas