Hi guys,

I've asked quotation for a component manufactured of ASTM A572 gr 50 with ENP. As I see, the steel is furnished without heat treatment or with stress relieving only, and here in our specification, we require a ENP with heat treatment at 600°C for 10hrs. I've checked A572 properties and it seems that this temperature can affect the material properties. Any recommendation to do it or not? Thank you!
 