May 9, 2014 #1 ironwoman Structural Joined May 9, 2014 Messages 1 Location GB Has this material been by a different ASTM #? Blueprint calling for this material spec was drawn in 1988. Can't find anything online. Thanks.
Has this material been by a different ASTM #? Blueprint calling for this material spec was drawn in 1988. Can't find anything online. Thanks.
May 9, 2014 #2 TVP Materials Joined Apr 12, 2002 Messages 4,592 Location US ASTM A570 has been withdrawn and replaced by ASTM A1011/1011M. Grade is still called Grade 33, same requirements. http://www.astm.org/DATABASE.CART/WITHDRAWN/A570A570M.htm Upvote 0 Downvote
ASTM A570 has been withdrawn and replaced by ASTM A1011/1011M. Grade is still called Grade 33, same requirements. http://www.astm.org/DATABASE.CART/WITHDRAWN/A570A570M.htm