Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations JAE on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

ASTM A53 Young's Modulus

Status
Not open for further replies.

Aton

Civil/Environmental
Joined
Mar 1, 2002
Messages
42
Location
CA
It has been several years since I have posted a question to this site. I am working in the Arctic and have been asked to design some small bridges for one of the commmunities here. As you may imagine, materials are extremely costly to ship up (once a year barge or flying in makes it all prohibitively expensive). In this particular community we have recently torn up some fuel pipelines - Schedule 40 pipe in long sections, and in good shape. The bridges are for over some seasonal creeks and deep gullies, and wiil be wide enough for only snow machines and All Terrain Vehicles. I am used to designing with standard structural steel, and am having great difficulty in finding the appropirate Young's Modulus to use for Schedule 40 pipe. I believe it is a steel with the characteristics very similar to AISI 1018, a mild steel. I am using conservative values: Yield Strength = 30 ksi Tensile Strength = 48 ksi. I believe that Young's Modulus should be similar to structural steel (29x10^6 psi). Does this sound right?

Sustainable, Solar, Environmental, and Structural Engineering: Appropriate technologies for a planet in stress.
 
Aton, don't have any reference available at this time, but 29 X 10^6 is going to be about right. It's just carbon steel.

Regards,

Mike
 
For ASTM A53, per ASME B31.3, Process Piping, the Elastic Modulus is:

30.2e6 @ -100 deg. F.
29.5e6 @ 70 deg. F.
28.6e6 @ 200 deg. F.

Good luck on those bridges.

NozzleTwister
Houston, Texas
 
Thanks, SnTMan, metengr, and NozzleTwister, for your help. I have been off-line for a time so could not answer. This is good info.
 
Status
Not open for further replies.

Part and Inventory Search

Sponsor

Back
Top