Does anyone know the DIN alternative of ASTM A440?

Thanks for your time...
 
EQUIVALENTS TO ASTM A440
BRITISH BS4360
INDIAN IS-961
RUSSIAN GOST 5058
GERMAN DIN 17100
JAPANESE JISG 5528

Have a good day, Rich
 