Jul 5, 2001 #1 Oz Mechanical Joined Jul 5, 2001 Messages 2 Location TR Does anyone know the DIN alternative of ASTM A440? Thanks for your time...
Jul 5, 2001 1 #2 Rich2001 Mechanical Joined Mar 23, 2001 Messages 896 Location US EQUIVALENTS TO ASTM A440 BRITISH BS4360 INDIAN IS-961 RUSSIAN GOST 5058 GERMAN DIN 17100 JAPANESE JISG 5528 Have a good day, Rich Upvote 0 Downvote
EQUIVALENTS TO ASTM A440 BRITISH BS4360 INDIAN IS-961 RUSSIAN GOST 5058 GERMAN DIN 17100 JAPANESE JISG 5528 Have a good day, Rich
Jul 6, 2001 Thread starter #3 Oz Mechanical Joined Jul 5, 2001 Messages 2 Location TR Thanks... Oz Upvote 0 Downvote