Hi

Can you please tell me the temperature range for ASTM A439 Austenitic Ductile Iron type D2? particularly interested in the minimum?

Thanks
 
Replies continue below

Recommended for you

Perhaps you can refer to the data provided by Ductile Iron Society.

Temperature Properties


"Properties and application of Ni Resist and Ductile Ni Resist alloys" NiDI publication.

The later publication recommends use of D2 iron upto -196C (-321F) with no remarkable drop in impact properties. Please refer to the TableXX Low TemperatureImpact Properties of some Spheroidal Graphite NiResist Alloys.
 