Hi,

Can anyone help me to find out the NACE MR0175 requirement for LF6 materials??
since this material is not listed in the NACE MR0175.

Dinu...

There are no secrets to success. It is the result of preparation, hard work, and learning from failure.
 
It doesn't have to be listed, it's a low alloy steel. Look under Part 2, Annex A, A.2.

Steve Jones
Corrosion Management Consultant


All answers are personal opinions only and are in no way connected with any employer.
 
If you see A.2.1.1 of NACE MR 0175, you find an answer.


(Quoted from A.2.1.1 of NACE MR 0175)

The majority of steels that comply with the general requirements of A.2 are not individually listed; however, for convenience, some examples of such steels are listed in Table A.2, Table A.3 and Table A.4.




Lee SiHyoung,
 