ASTM A325 specs states that the minimum tensile strength be 120 ksi for bolts from 1/2" to 1" and 105 ksi for diameters 1 1/8" thru
1 1/2"
AISC 360-05 states the nominal tensile stress for A325 bolts as 90 ksi, presumably from 0.75 Fu.

It states this exclusive of bolt size.

Why do the larger diameter bolts not have a lower nominal tensile stress = 0.75Fu or 0.75*105ksi = 79 ksi in order to correspong to the ASTM spec?
 
Replies continue below

Recommended for you

Look at the fourth paragraph in the AISC 360 commentary in your 13th edition manual (page 16.1-344).

 
Hmmm...pretty straight forward.
I guess I should have read the commentary before I wasted time posting.

Thanks JAE
 