Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations cowski on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

ASTM A262 rapid screening test

Status
Not open for further replies.

cv1

Materials
Jan 23, 2001
11
The rapid screening test suggests an applied voltage of 20V. If the current density is achieved for the sample size does the voltage applied have any significant effect? or will any reasonable voltage less than 20V still achieve an acceptable result?

Any suggestions or thoughts would be appreciated.
 