What does the "WPBN" represent?

I have a fitting with...A/SA234 WPBN W8297 GT...stamped on it? Can anyone describe what all that represents?
 
Replies continue below

Recommended for you

OK...What about the "WPB" and "W8297"?
 
WPB means fitting made of carbon steel grade B , See ASTM A 234.
W8297GT could be the Heat #
 