I am looking URGENTLY for ASTM A217 GR. C5 gate valves 6". Could any one inform me from where I can get the valves from stock. This is an urgent requirement for my clients shut down. Please advise ASAP.
 
Replies continue below

Recommended for you



.....where are you, how many, operator (handweel, gear or actuator type), any particulars on coating, certificates, tests, flangeforms etc?

Your case is a normal purchasing case, but you will not get very sensible answers anywhere if you do not tell exactly what you want.

PS. Should not be that difficult anyway, some stockists specialize in keeping items in stock for short delivery. If price and transport costs does not matter, try European stockists for Northsea offshore. If too far away try nearest offshore supply centers.



 
dear gerhardl (Mechanical),

below is the specification, qnty: 16 pieces. please suggest me a good stockist ASAP as I require this for an urgent shutdown

VALVE, GATE, CLASS 300, FLANGED, RAISED FACE, BODY MATERIAL ALLOY STEEL TO ASTM A217 GR. C5,
TRIM No. 2, STEM, DISC AND SEAT TO ASTM A182 GR. F.304, OPERATING TEMPERATURE: 650 DEG. F.
FLUID SULPHUR CONTENT: 5.1%.
SIZE IN INCHES: 6
DESIGN SPEC: API 600
PACKING STEM: JOHN CRANE 287-1 OR EQUAL
 
Your problem is probably the high temperature requirement together with building length/flanges and material spec.

Phoning nearest representative below for advice could perhaps bring you a step further, if you have not been able to progress on your own already.

 
Dear ValveSteve,

This is urgently required. no time to fabricate
 

... agree with ValveSteve. Some companies specializes in fabricating (often from barstock) within a few days. It will cost, but it is a possibillity.


 
Was this issue resolved successfully? If so, could you share where you were able to purchase this quantity of c5 valves from stock?
 