The ASTM A193-B8M, Class 2 spec calls out a solution anneal and cold drawn material. The cold work is what kicks up the tensile strength on this material. Is there a way to tell how deep the cold work goes in the material when it is cold drawn? I have a customer who wants to machine some B8M, Class 2 material but is afraid he will machine all of the cold work off of the bar (he would be machining about 1/2" off a side). I told him that I am not 100% sure but think that would be enough to remove the cold work applied during the drawing process. Is there a way to tell how deep the cold work is applied to this material during the drawing process?