I have the following question, who can help me please?
We have to supply forgings according to ASTM A182, complete certified including supplementary requirement S6, which is a hardness test.
Quote: "S6.1 Each forging shall be hardness tested and shall meet the requirements of Table 3."
Literal, when we have a batch of 1,000 equal sizes forging, of the same heat, produced in a same continues run, we have to test all 1,000 forging each on hardness.
Is my interpretation correct?
If so, what is the reason for this 100% check, because all forgings have suffer the same treatment, so all test results shall show the same results.
Besides, it will push up the price of the product.
Thank you.
We have to supply forgings according to ASTM A182, complete certified including supplementary requirement S6, which is a hardness test.
Quote: "S6.1 Each forging shall be hardness tested and shall meet the requirements of Table 3."
Literal, when we have a batch of 1,000 equal sizes forging, of the same heat, produced in a same continues run, we have to test all 1,000 forging each on hardness.
Is my interpretation correct?
If so, what is the reason for this 100% check, because all forgings have suffer the same treatment, so all test results shall show the same results.
Besides, it will push up the price of the product.