Oct 15, 2009 #1 lizardtoe Mechanical Joined Oct 15, 2009 Messages 1 Location US What are the differences in the two grades of piping. I am specifically interested in corrosion resistance characteristics. thanks!
What are the differences in the two grades of piping. I am specifically interested in corrosion resistance characteristics. thanks!
Oct 16, 2009 #2 metengr Materials Joined Oct 2, 2003 Messages 15,478 Location US Corrosion resistance would be roughly the same for bare pipe supplied by both specifications. ASTM A 53 offers galvanized pipe as an option for corrosion protection versus A 135. Upvote 0 Downvote