ASTM A-487 GR 9-A,B,C,D Casting only???

Status
Not open for further replies.

eddiewdi

Mechanical
Jun 28, 2006
15
Is ASTM A-487 GR 9-A,B,C,D for casting only or can this spec be applied to forge material also?
 
Replies continue below

Recommended for you

No. ASTM A 487 is only applicable to cast product forms.
 