Nov 8, 2010 #1 TeejT Mechanical Joined Jan 19, 2010 Messages 80 Location CA Does anyone have the ID tolerance spec on 1-1/4" SCH 40 pipe? Thanks!
Nov 8, 2010 #2 metengr Materials Joined Oct 2, 2003 Messages 15,478 Location US Don't double post. Upvote 0 Downvote
Nov 8, 2010 Thread starter #3 TeejT Mechanical Joined Jan 19, 2010 Messages 80 Location CA It falls under an ASTM standard and an ASME standard... Upvote 0 Downvote
Nov 10, 2010 #4 EdStainless Materials Joined May 20, 2004 Messages 16,351 Location Waukesha WI USA There is no ID tol. Only OD and wall tol. You can see the total combined, and on pipe that is a big number. The max wall on pipe is only limited by weight, so heavy pipe is a possibility. = = = = = = = = = = = = = = = = = = = = Plymouth Tube Upvote 0 Downvote
There is no ID tol. Only OD and wall tol. You can see the total combined, and on pipe that is a big number. The max wall on pipe is only limited by weight, so heavy pipe is a possibility. = = = = = = = = = = = = = = = = = = = = Plymouth Tube