Jun 15, 2011 #1 cezarcbc Industrial Joined Jan 19, 2011 Messages 4 Location BR If I have two plates in stainless steel cladded on carbon steel plate. Is it necessary to test specimens of two stainless steel plates for mechanical testing to qualify to ASTM-A-264?
If I have two plates in stainless steel cladded on carbon steel plate. Is it necessary to test specimens of two stainless steel plates for mechanical testing to qualify to ASTM-A-264?
Jun 15, 2011 #2 metengr Materials Joined Oct 2, 2003 Messages 15,478 Location US Do you have a copy of ASTM A 264?????? Review 7.0. Upvote 0 Downvote
Jun 15, 2011 Thread starter #3 cezarcbc Industrial Joined Jan 19, 2011 Messages 4 Location BR I have a copy of the standard, I am in doubt in paragraph 8.1 Upvote 0 Downvote
Jun 15, 2011 #4 metengr Materials Joined Oct 2, 2003 Messages 15,478 Location US I reviewed 8.1 this discusses the possibility of product analysis as it applies to the cladding material itself. Read on to 8.2. Upvote 0 Downvote
I reviewed 8.1 this discusses the possibility of product analysis as it applies to the cladding material itself. Read on to 8.2.