Sep 24, 2007 #1 WeldGk Materials Joined Aug 14, 2007 Messages 42 Location CA Is there a cast equivalent for ASTM A105? The closest I can match is ASTM A352, LCC.
Sep 24, 2007 #2 gr2vessels Mechanical Joined Sep 29, 2004 Messages 1,971 Location AU I would rather suggest the ASTM A216, not the A352. cheers, gr2vessels Upvote 0 Downvote