Hi,
our tank manufacturer wants to change the tank material from specified ASTM 285 Gr.C to ASTM A36. The affected storage tanks are atmospheric and on the one hand for PHC sludge covered by API 650, diameter from 2000 to 5500 mm and on the other hand water tanks covered by AWWA D100 from 5500 to 12500 mm.
As far as I know all the applicable codes deal with A36 but I'm not familiar if there are any restrictions for this material. Can anybody teach me ?
best regards
Jens Binder
our tank manufacturer wants to change the tank material from specified ASTM 285 Gr.C to ASTM A36. The affected storage tanks are atmospheric and on the one hand for PHC sludge covered by API 650, diameter from 2000 to 5500 mm and on the other hand water tanks covered by AWWA D100 from 5500 to 12500 mm.
As far as I know all the applicable codes deal with A36 but I'm not familiar if there are any restrictions for this material. Can anybody teach me ?
best regards
Jens Binder