Resent ILI data shows that 75% Wt loss for 10mm x 15mm area for a API 5L X52 (7.9 mm thick)
Gas pipe line. As per the effected area method calculation this defect can be attended by blasting the surface and by applying epoxy coating to the surface. Apart from coating for an in service pipe line, is there any other method to rectify this wall loss defect? Can we go step further and have a type A sleeve repair by using clock spring?
Gas pipe line. As per the effected area method calculation this defect can be attended by blasting the surface and by applying epoxy coating to the surface. Apart from coating for an in service pipe line, is there any other method to rectify this wall loss defect? Can we go step further and have a type A sleeve repair by using clock spring?