Dear All,
We have a concrete deck paved with asphalt wearing course 50mm thick. There is a 4mm thick waterproofing membrane between the concrete deck and the BWC. Due to the debonding effects and low compaction, some of the paved areas are cracked.
What is the best solution to fix-up these cracks? Whether to cut the 50mm asphalt and putback the membrane and re-lay the asphalt or to fill these cracks with a bituminous grout?
The crack width is 2mm approx.
Please help...
We have a concrete deck paved with asphalt wearing course 50mm thick. There is a 4mm thick waterproofing membrane between the concrete deck and the BWC. Due to the debonding effects and low compaction, some of the paved areas are cracked.
What is the best solution to fix-up these cracks? Whether to cut the 50mm asphalt and putback the membrane and re-lay the asphalt or to fill these cracks with a bituminous grout?