Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations TugboatEng on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

ASME X vx BS 9449

Status
Not open for further replies.

tr6

Mechanical
Joined
Oct 2, 2002
Messages
81
Location
US
What are the significant differences in design, materials, fabrication, and testing between ASME X and BS 9449? Is one generally more rigerous and/or expensive to meet?

Our company is generally involved in the fabriction of metallic pressure vessels and has no experience in FRP/Composite pressure vessels.

Thanks for your responses.
 
One code is for pressure vessels, the other is for tanks (not pressure vessels). Apart of that, there are many similarities, like the use of the fibreglass reinforced plastic.
Howzat,
cheers,
gr2vessels
 
It's been many years since I dealt with FRP.

FRP is not as easily inspected as steel. You cannot perform a volumetric analysis of a secondary bond the same way as you can perform a radiograph of a weld. The quality control side of things is much more complex as a steel tank or pressure vessel may have 20 "parts" which you trace heat numbers where an FRP tank may have 1000 different pieces of glass.

To answer your questions above relative to the differences between steel and FRP:

Design - steel is essentially the same in all directions, FRP you tailor the properties of the laminate to the directions where you need the strength.

Materials - steel is provided with a mill test report that states chemistry, tensiles etc. FRP you may get some information on the glass and the resin but the end properties depend on how you put the two together.

Fabrication - It's been a while but I believe that ASME X requires some type of qualification for secondary bonders. If it does not it would be a good idea to perform some type of qualification test. That way you have proof that the people doing the work are good at it.

Testing - For steel there is radiography, dye penetrant, and others. FRP there is visual, accoustic emission, visual, and more visual. The importance with FRP is to have skilled inspectors who know what to look for with FRP laminates.

I am not familiar with BS 9449 so I cannot comment on how it compares to what I have mentioned above.