Dear All,
I have to buy eleven air coolers in which the bundle is designed as per follow conditions:
-Design Pressure of 325 bars (g)
- Temperature design of 90°C
The material proposed, during the bid phase, from different Vendors is a Super Duplex Type 2507 in order to be in line with the process fluid chemical composition (recycle water with high chloride content).
Considering the above case, I would like to ask you some questions:
1) Could be better to design the Tube Bundle in accordance with ASME VIII Div.2 instead of Div.1?
In terms of headers thickness surely yes, but which are the negative side using the Div.2?
2) Are there other header types which could be employed for this purpose, considering that the actual offers are based on plug and pipe types headers?
3) Using a pipe type header can be the cleanness of tubes provided only if the bundle is one pass?
Any answer or other information on the matter would be greatly appreciated.
Thank you in advance,
Bye bye
I have to buy eleven air coolers in which the bundle is designed as per follow conditions:
-Design Pressure of 325 bars (g)
- Temperature design of 90°C
The material proposed, during the bid phase, from different Vendors is a Super Duplex Type 2507 in order to be in line with the process fluid chemical composition (recycle water with high chloride content).
Considering the above case, I would like to ask you some questions:
1) Could be better to design the Tube Bundle in accordance with ASME VIII Div.2 instead of Div.1?
In terms of headers thickness surely yes, but which are the negative side using the Div.2?
2) Are there other header types which could be employed for this purpose, considering that the actual offers are based on plug and pipe types headers?
3) Using a pipe type header can be the cleanness of tubes provided only if the bundle is one pass?
Any answer or other information on the matter would be greatly appreciated.
Thank you in advance,
Bye bye