Dear All,
Can someone help me in this matter.
Equipment: Sphere
Design Code: ASME VIII Div.1
Shell thickness: 50.4 mm
PQR qualified according to ASME IX:
Material: SA 537 Cl 1
Coupon thickness: 32mm
Impact Test: YES
PWHT Holding Time: 240 minutes (4hr) (We planned this time to be able to do a 2nd PWHT if there is any repairs and for maintenance after the 1st PWHT).
WPS:
Material: SA 537 Cl 1
Thickness range: 16 to 64 mm
PWHT Minimum Holding Time : 120 minutes according to ASME VIII Div.1 Table UCS-56-1.
Our client rejected the WPS and requested that the Minimum Holding Time should be 135 minutes instead of 120 minutes as per Table UCS-56-1 [2 hr plus 15 min for each additional inch (25 mm) over 2 in. (50 mm)].
Note that Standard Units used are SI millimeters (mm)
In my understanding "15 min for each additional 25 mm over 50 mm" means:
50 mm + 25 mm = 75 mm ------------------------------> + 2hr 15 min = 135 min
50 mm + 25 mm + 25 mm = 100 mm ---------------------> + 2hr 15 min + 15 min = 150 min
50 mm + 25 mm + 25 mm + 25 mm = 125 mm -------------> + 2hr 15 min + 15 min + 15 min = 165 min
In our case the thickness is 50.4 mm, it has not reached 75 mm, so the minimum holding time should be 120 minutes and not 135 minutes !
Am I right or wrong?
Please, enlighten me on the subject because I have to answer as soon as possible to our client.
Thanks in advance
Can someone help me in this matter.
Equipment: Sphere
Design Code: ASME VIII Div.1
Shell thickness: 50.4 mm
PQR qualified according to ASME IX:
Material: SA 537 Cl 1
Coupon thickness: 32mm
Impact Test: YES
PWHT Holding Time: 240 minutes (4hr) (We planned this time to be able to do a 2nd PWHT if there is any repairs and for maintenance after the 1st PWHT).
WPS:
Material: SA 537 Cl 1
Thickness range: 16 to 64 mm
PWHT Minimum Holding Time : 120 minutes according to ASME VIII Div.1 Table UCS-56-1.
Our client rejected the WPS and requested that the Minimum Holding Time should be 135 minutes instead of 120 minutes as per Table UCS-56-1 [2 hr plus 15 min for each additional inch (25 mm) over 2 in. (50 mm)].
Note that Standard Units used are SI millimeters (mm)
In my understanding "15 min for each additional 25 mm over 50 mm" means:
50 mm + 25 mm = 75 mm ------------------------------> + 2hr 15 min = 135 min
50 mm + 25 mm + 25 mm = 100 mm ---------------------> + 2hr 15 min + 15 min = 150 min
50 mm + 25 mm + 25 mm + 25 mm = 125 mm -------------> + 2hr 15 min + 15 min + 15 min = 165 min
In our case the thickness is 50.4 mm, it has not reached 75 mm, so the minimum holding time should be 120 minutes and not 135 minutes !
Am I right or wrong?
Please, enlighten me on the subject because I have to answer as soon as possible to our client.