Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations MintJulep on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

ASME VIII Div.1 Annex 2 Bolting Cross-Sectional Area: “nominal stress area” ??

Status
Not open for further replies.

Henzy1977

Mechanical
Joined
May 8, 2019
Messages
7
Location
NL
ASME VIII Div.1 Annex 2 2-3 (Notation) specifies the following definition for Am1/Am2: “total cross‐sectional area of bolts at root of thread or section of least diameter under stress”.

I have a to verify a body-bonnet connection of a valve with Annex 2 and the connection is performed using Socket Head Cap Screws. Can I use the ISO value of the “nominal stress area” instead of the root of thread area?

Is it possible to say that for screws ( e.g. Hex Type ) the least diameter under stress can be the nominal stress area even if it’s value is bigger than the root area?

Thanks
 
No, not as far as I'm aware. Appendix 2 calculations require you to use the root area of the bolt, not the effective tensile area.

If possible, you may want to consider using larger diameter or higher strength bolts. Another way to increase the root area is to specify fine thread (UNF) bolts.


-Christine
 
I think in ASME VIII and EN 13445 (pressure vessels) you must always use the root area of bolting.

Best regards
 