May 12, 2021 #1 KevinNZ Mechanical Joined Jun 12, 2003 Messages 868 Location NZ Hi all What the value for C from UG-34 to use when the flat head extends past the shell and is welded from the outside only.
Hi all What the value for C from UG-34 to use when the flat head extends past the shell and is welded from the outside only.
May 13, 2021 #2 TGS4 Mechanical Joined Nov 8, 2004 Messages 3,985 Location CA As you are aware (hence your question), this detail is not covered by UG-34(d) and not included in Figure UG-34. I would revert to U-2(g). Upvote 0 Downvote
As you are aware (hence your question), this detail is not covered by UG-34(d) and not included in Figure UG-34. I would revert to U-2(g).
May 13, 2021 #3 david339933 Industrial Joined Jun 15, 2011 Messages 1,204 Location CA Which leads to the question....Why are details included in Fig. UW-13.2, but not in UG-34? Upvote 0 Downvote
May 13, 2021 3 #4 cbPVme Mechanical Joined Sep 21, 2015 Messages 73 Location CA How about C=0.33 per Figure UG-34 sketch (h)? This directly references Figure UW-13.2 sketches (a) to (g). Upvote 0 Downvote
How about C=0.33 per Figure UG-34 sketch (h)? This directly references Figure UW-13.2 sketches (a) to (g).
May 14, 2021 Thread starter #5 KevinNZ Mechanical Joined Jun 12, 2003 Messages 868 Location NZ Thanks cbPVme Upvote 0 Downvote