My first post ever - though I've been lurking around for quite a while - and it is a question.
Why isn't wrought aluminum 7075 (A97075) and any of its tempers listed on the ASME stress tables?
I need a small pressure vessel to withstand 6500psi at 40ºC. The vessel will act as a sample holder in a tomograph, so the vessel material has to be aluminum in order to not interfere with the analysis.
The mechanical engineers say they can not design the vessel using Al7075 simply because this alloy is not listed on the ASME stress tables, hence my question.
Thank you.
Why isn't wrought aluminum 7075 (A97075) and any of its tempers listed on the ASME stress tables?
I need a small pressure vessel to withstand 6500psi at 40ºC. The vessel will act as a sample holder in a tomograph, so the vessel material has to be aluminum in order to not interfere with the analysis.
The mechanical engineers say they can not design the vessel using Al7075 simply because this alloy is not listed on the ASME stress tables, hence my question.
Thank you.