Horserider22
Mechanical
Hello
I`m new to ASME IX
A complete joint penetration PQR was done with SMAW on 1/4" thick material, it is qualified for base metal thickness up to 2T so 1/2" thick. QW-202.2(C) For fillets weld: all base metal thicknesses and all fillet sizes.
I now need to fillet weld some attachments that are 1 inch thick. Does this mean that my maximum plate thickness is 1/2" for fillet welds or do fillet weld have a unlimited material thickness meaning I could weld some attachments plates that are 6" thick.
Thanks for your time
I`m new to ASME IX
A complete joint penetration PQR was done with SMAW on 1/4" thick material, it is qualified for base metal thickness up to 2T so 1/2" thick. QW-202.2(C) For fillets weld: all base metal thicknesses and all fillet sizes.
I now need to fillet weld some attachments that are 1 inch thick. Does this mean that my maximum plate thickness is 1/2" for fillet welds or do fillet weld have a unlimited material thickness meaning I could weld some attachments plates that are 6" thick.
Thanks for your time