Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations TugboatEng on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

ASME section II part D - differences in listed materials between M & USC version

Status
Not open for further replies.

XL83NL

Mechanical
Joined
Mar 3, 2011
Messages
3,120
Location
NL
I was going in depth in ASME BPVC II-D:2017, both the metric & US (customary) version. For table 1A, I found that the notes between both versions arent the same; review notes H6 & H7 of table 1A for the USC version. Upon further review, by going through table 1A to see where the notes are applicable, I found that the USC version includes H6, which reads
Material shall be solution annealed at 2010°F to 2140°F, followed by a rapid cooling in water or air.
This note isnt found in the metric version.

Note H6 of the USC version is applicable to
[ul]
[li]Page 82, lines 3 & 4; SA-240 UNS S30601[/li]
[li]Page 114, lines 25 ÷ 34; SA-182/240/312/479 UNS S30600[/li]
[li]Page 114, lines 43 ÷ 46; SA-213/240 UNS S32615[/li]
[li]Page 118, line 1 ÷ 4; SA-312/479 UNS S32615[/li]
[/ul]
These materials arent found in table 1A, metric edition. Why does the code has different materials in the codes, if the user is free to go for either the metric ro US customary version?
 
Likely an oversight. Please submit an inquiry to the Section II Code Committee (secretary).
 
Thanks TGS4, will do so.
 