Apr 5, 2012 #1 ASA7 Materials Joined Apr 5, 2012 Messages 1 Location GB Are the materials listed below suitable for use as pressure bounding material according to the ASME BPVC Section II, Section A? ASTM 1020 ASTM 106 API 5L, Grade B ASTM 516
Are the materials listed below suitable for use as pressure bounding material according to the ASME BPVC Section II, Section A? ASTM 1020 ASTM 106 API 5L, Grade B ASTM 516
Apr 5, 2012 #2 stanweld Materials Joined May 9, 2003 Messages 2,906 Location US No. ASTM A-1020 and API 5L are not listed in Section II. ASTM A-106 and A-516 may be if they are SA-106 and SA-516 as defined in Section II. Upvote 0 Downvote
No. ASTM A-1020 and API 5L are not listed in Section II. ASTM A-106 and A-516 may be if they are SA-106 and SA-516 as defined in Section II.
Apr 5, 2012 #3 metengr Materials Joined Oct 2, 2003 Messages 15,478 Location US Not all materials listed in Section II, Part A or B are permitted for use in pressure boundary applications. The materials permitted for use are in Section II, Part D, where allowable stress lines are provided for material specification and grade. Upvote 0 Downvote
Not all materials listed in Section II, Part A or B are permitted for use in pressure boundary applications. The materials permitted for use are in Section II, Part D, where allowable stress lines are provided for material specification and grade.