Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations LittleInch on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

ASME section 1, year 2011, table PW-11 volumetric examination, interpretation

Status
Not open for further replies.

Roger00

Mechanical
Joined
Apr 9, 2008
Messages
18
Location
ID
Hi All,

Please share your opinion. can UT replace RT for tubes subject to furnace radiant heat with diameter below NPS 4 (DN 100) and thickness below 0.5 in. (13 mm). ASME Section I, 2011, table PW-11, general notes (g), requires thickness below 0.5 in shall be RT, while in the table for tubes requires volumetric examination if OD above NPS 4 and thickness above 0.5 in. I have read code case 2235, year 2005, UT can replace RT for thickness at 13 mm and greater.

second question, If tubes has OD below NPS 4 and thickness is below 0.5 in, is volumetric inspection required?