ASME sect. IX qualified a PQR with a T joint for fillet weld according to QW-451.3

Status
Not open for further replies.

LouisLac

Materials
May 5, 2012
23
Hi,

If I qualified a PQR for fillet weld (T-Joint, QW-451.3) without toughness, can I use this to weld a part with a toughness requirement?

Thanks
 
Replies continue below

Recommended for you

@louis lac, a PQR qualified without toughness cannot be used for a weld with toughness, regardless of whether the coupon/job is a fillet weld or a groove weld.
 